Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEW PRODUCTS
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • MAX
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
Adhesives and Sealants TopicsCoatingsFinished Adhesives and SealantsRaw Materials and ChemicalsTesting/Quality Control

Top 5 News that Sticks

3M Acquisition Dominates the News

Readers last week were drawn in droves to news from 3M regarding its latest acquisition.

By Susan Sutton
October 28, 2019

Readers last week were drawn in droves to news from 3M regarding its latest acquisition (3M Completes Acelity Acquisition): “3M recently announced that it has completed its acquisition of Acelity, Inc. and its KCI subsidiaries worldwide for a total enterprise value of approximately $6.7 billion, including assumption of debt and other adjustments. Acelity produces KCI-branded products for advanced wound care and specialty surgical applications.

“‘This is an exciting day as we bring together two premier and innovative companies that are focused on delivering comprehensive health care solutions to enable better outcomes for patients,’ said Mike Roman, 3M chairman and CEO. ‘We are excited to have the tremendous people of Acelity join the 3M team, and are confident in the value that this acquisition will deliver to our customers and our shareholders. This addition further accelerates 3M as a leader in advanced wound care, which is a significant and growing market segment.’”

We’ve seen a large number of industry acquisitions so far in the second half of 2019. How are they impacting your business?

Top 5 News that Sticks for October 20-26

  1. 3M Completes Acelity Acquisition
  2. IGM Resins Outlines Growth Strategy for Energy Curing Resins Business
  3. Industrial Caulk and Seal Completes 1 Million Linear Feet of Joint Fill
  4. BYK Announces Management Change as Glander Steps Down
  5. AkzoNobel to Supply Coatings for New York Yacht Club’s American Magic Team

This weekly roundup highlights the adhesives, sealants, and coatings-related news stories that garnered the most attention during the previous week on our website, as well as our eNewsletters and social media platforms.

KEYWORDS: acquisitions adhesives in medical/dental caulks marine coatings personnel resins and base polymers

Share This Story

Susan sutton 200px

Susan Sutton is the former Editor-in-Chief of Adhesives & Sealants Industry.

Blog Topics

Editor's Blog

Survey Says!

Adhesives & Sealants Around the Web

Recent Comments

I recommend you to try https://edureviewer.com/services/quizplus-review/ ....

I think that you are right, now there...

You are right, now people have begun to...

Good experience after reading. In fact, now many...

Good idea, although I'm now increasingly shopping online,...

Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Popular Stories

henkel

FTC Sues to Block Henkel-Liquid Nails Acquisition, Citing Antitrust Concerns

2025 CASE eBook

The 2025 PCI/ASI CASE eBook

Man reading news on tablet

EPA Announces Intent to Regulate Phthalate Chemicals Used in Adhesives and Sealants

ASI Top 20 website

Events

January 15, 2026

From Data Silos to AI Success: Lessons from Collano’s Journey

In this webinar, Raphael Schaller, CTO of Collano, shares how his team envisioned their data to make it usable for AI-driven materials discovery. He reflects on what he would do differently if starting over, and how adopting the Citrine Platform has accelerated learning, collaboration, and innovation across the organization.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

ASI CASE EBOOK

ASI webinar

×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing