Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Adhesives Mag logo
  • NEWS
    • Latest Headlines
    • ASI News Now
    • Mergers/Acquisitions
    • Market Trends
    • TOP 20
  • NEW PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • From the Editor
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • EVENTS
    • ASI Academy
    • Events Calendar
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Sponsor Insights
    • Classifieds
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
    • CONTACT
  • SIGN UP!
Home » sealants in transportation

Articles Tagged with ''sealants in transportation''

Photo of a sticky note with drawing of a lightbulb

DOW: Self-Adhesive Liquid Silicone Rubber

January 12, 2023

The SILASTIC SA 994X LSR series is a range of primerless, self-adhesive, general purpose, and self-lubricating, one-to-one mix ratio liquid silicone rubbers (LSRs) designed for two-component injection molding with thermoplastic substrates including, but not limited to, polybutylene terephthalate and polyamide.


Read More
scale

Adhesives for Lightweighting of Structures—Drivers, Selection, Challenges

Lightweighting of structures and combining of materials to take advantage of their best properties is becoming a part of engineering design, and adhesives will play an increasing role in those future designs and applications.
George Ritter
George W. Ritter, Ph.D.
October 27, 2022

Lightweighting of structures is most often associated with automotive structures. However, lightweighting is a challenge across the transportation sector, including trucks, trailers, buses, passenger rail cars, and even heavy earth-moving equipment and cranes.


Read More
Ford Blue Oval City

Ford to Build New Electric Vehicle Mega-Campus in Tennessee, Battery Plants in Kentucky

The facilities will produce the next generation of electric F-Series trucks and the batteries to power future electric Ford and Lincoln vehicles.
September 30, 2021
Ford Motor Co. recently announced plans to bring electric vehicles at scale to American customers with two new environmentally and technologically advanced campuses in Tennessee and Kentucky.
Read More
New-Prods

CREATIVE MATERIALS: Coating and Encapsulant

Applications include electronics, automotive manufacturing, shipbuilding, aerospace, military, and telecommunication.
September 28, 2021
Creative Materials recently introduced 111-27, an electrically insulating, thermally curing, colorless coating and encapsulant that can be applied by different methods.
Read More
electric cars

Arkema Acquires Stake in Battery Producer Verkor

Arkema contributed several million euros to Verkor’s recent €100 million (approximately $118.7 million) round of fundraising.
July 14, 2021
Arkema recently announced that it has become a shareholder and technological partner of Verkor, a French startup specializing in the production of high-performance batteries.
Read More
Master Bond low-outgassing epoxy

MASTER BOND: Low-Outgassing Epoxy

As a toughened system, this epoxy resists thermal cycling and is ideal for bonding dissimilar substrates.
June 22, 2021
Master Bond Supreme 70CN is a two-part epoxy adhesive formulated using a natural, renewable, and sustainable ingredient.
Read More
Fig1
Strategic Solutions

Market Dynamics for North American Sealants

Through 2019, the building and construction market was a sealants volume leader, followed by assembly operations and transportation.
AggieLotz.jpg
Aggie Lotz
August 17, 2020

The wide use of dissimilar substrate materials driving the selection of sealants was reported in The Adhesive and Sealant Council’s “2017-2020 North American Market Report for Adhesives and Sealants with a Global Overview.”


Read More
airplane interior
Product Profile

B-Staged Epoxy Meets Airbus Standards for Flame Retardancy and Toxicity

Adhesives and sealants must meet stringent requirements for use in aircraft and other applications.
June 17, 2020
Master Bond EP36FR is a specialized one-part epoxy that meets Airbus specifications for toxic gas emissions per AITM 3.0005, Issue 2 in the flaming mode and Section 7.4 of ABD0031, Issue F.
Read More
transportation adhesives

SIKA CORP.: Easy-to-Remove Elastic Butyl Sealant

Recommended applications for SikaLastomer-714 include the sealing of bolt-in parts to vehicle flanges (i.e., truck sliders), as well as the sealing of gaskets to various substrate materials.
March 12, 2020

Sika Corp. recently introduced its SikaLastomer-714 butyl sealant for the U.S. transportation aftermarket. 


Read More
Market-Trends

Luxury Vehicle Market to See Strong Growth through 2023

Increasing demand for luxury vans and buses, as well as electrified vehicles, is positively impacting the market.
June 17, 2019

A recent market research study projects the global luxury vehicle market to grow at a CAGR of more than 12% from 2019-2023.


Read More
Previous 1 2 3 Next
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Industrial robot performing plasma surface treatment on an automotive component
    Sponsored byPlasmatreat North America

    Engineering the Molecular Interface: Atmospheric Plasma Cleaning and Activation for Reliable Bonding

  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

news on internet screen

Sika Closes Acquisition of Akkim

Image of green tree within clear lightbulb

Researchers Develop a Reusable Adhesive from Waste Polymers

image of a graph representing markets

Pricing, Restructuring Savings Drive H.B. Fuller Q3 Growth

ASI 2026 Top 20 Adhesives & Sealants List

Events

October 5, 2026

Polyurethanes Technical Conference

The Polyurethanes Technical Conference, hosted by the American Chemistry Council’s Center for the Polyurethanes Industry (CPI), will feature educational sessions and the latest innovations in polyurethane chemistry.

October 12, 2026

The Battery Show Detroit 2026

Join 16,000+ engineers, executives, and innovators for four days of hands-on learning, strategic networking, and direct access to the technologies shaping the future of batteries and EVs.

View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing