Henkel Loctite Corp. has introduced two fluorescent FLASHCURE light curing cyanoacrylates designed for the assembly of components where the ability to verify the presence of the applied adhesive is desired.
UM25 Series Universal modules from Nordson Corp. provide accurate hot melt adhesive dispensing in a single-platform design to simplify in-house rebuilding and reduce maintenance and inventory costs.
Researchers at the Department of Energy's Sandia National Laboratories in Livermore, CA, have developed a high-temperature, high-strength structural support foam, TEPIC, that has proven to be an exceptionally versatile material for use as molded-to-shape models as well as prototype and production run tooling for composites manufacturing.
ATS RheoSystems has introduced its new STRESSTECH HR Rheometer equipped with novel UV Cure Monitoring Accessory and proprietary Fast Oscillation Data Acquisition Software.
BBA Fiberweb Filtration has completed the development of DiamondWeb - a new spunbond polyester filtration media - following an investment of proprietary technology and process design.
A new selector guide from DYMAX Corp. features a wide range of materials for electronic and electo-optical assembly, as well as a selection of compatible light-curing equipment.