    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • EVENTS
    • ASI Academy
    • Events Calendar
  • COLUMNS
    • European Perspectives
    • Strategic Solutions
    • Supply Chain Strategies
    • Tape Talk
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Webinars
    • eBooks
  • EXPLORE
    • Adhesives in Action
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
    • Classifieds
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
  • EMAGAZINE
    • EMAGAZINE
    • ARCHIVE ISSUES
    • ADVERTISE
      • Custom Content & Marketing Services
    • CONTACT
  • SIGN UP!
NewsAdhesives and Sealants TopicsAdhesives & Sealants HeadlinesRaw Materials and Chemicals

SOCMA Welcomes New Members to Its Board of Governors

audience clapping
February 9, 2023

The Society of Chemical Manufacturers & Affiliates (SOCMA) announced its 2023 board of governors, including six new board members and a new slate of executive officers. The association’s leadership is composed of senior industry executives representing diverse capabilities across the specialty and batch chemical manufacturing sector. SOCMA also welcomes Kate Hampford Donahue, president and CEO of Hampford Research Inc., who will serve a two-year term as chair of the association’s board, spanning 2023-2024.

“SOCMA has been vital to the growth and success of my own company over many years, and I am honored to take over the chairmanship of the leading voice for the specialty and batch chemical industry,” said Donahue. “As companies across our sector navigate a demand-driven yet shifting landscape, I am committed to stewarding programs that maximize member visibility and strengthen manufacturing operations.”

“I am proud to work alongside Kate and this extremely knowledgeable group of industry leaders who make up SOCMA’s 2023 board of governors,” said Jennifer Abril, SOCMA president and CEO. “As we launch into an unpredictable year, I look forward to the benefit of the board’s effective guidance and executable know-how which will continue to catapult SOCMA forward.”

Officers newly appointed to the executive committee include:

  • Chair – Kate Hampford Donahue, Hampford Research Inc.
  • 1st vice chair – Mara Gliozzi, McGean
  • 2nd vice chair and Treasurer – Charles Hinton, Ph.D., Ethox Chemicals
  • Secretary – Kenneth Zrebiec, Veranova
  • Member-at-large – John Zuppo, Ascent Chemicals
  • Immediate past chair – Michael Ott, Polysciences Inc.

Members of the board of governors’ class of 2025 include:

  • Jeana Beeland, CJB Industries
  • Alan Dyke, Ph.D., Boulder Scientific Co.
  • Sandra Cernick, Pressure Chemical
  • David Anderson, Colonial Chemical
  • Eric Lookofsky, CHEM Group
  • Todd Zahn, American Chemical Solutions


For more information, visit: www.socma.org.

KEYWORDS: associations feedstocks personnel resins and base polymers

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • 2026 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    2026 ASI Top 20: Leading Global Adhesives and Sealants Manufacturers

    Every year, we study the leading worldwide manufacturers...
    Pressure-Sensitive Adhesives (PSAs)
    By: Karen Parker
  • PSA Market

    Trends and Opportunities in Pressure-Sensitive Adhesives: Sustainability, Innovation, and Market Growth

    The pressure-sensitive adhesives market is growing...
    Pressure-Sensitive Adhesives (PSAs)
    By: Chirag Tripathi and Parag Shah
  • science test tubes

    2026 Adhesives and Sealants Raw Materials Roundup

    After more than two years of contraction, the...
    Raw Materials and Chemicals
    By: Karen Parker
Manage My Account
  • eMagazine Issues
  • Newsletters
  • Online Registration
  • Manage My Preferences
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Adhesives and Sealants Industry audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Adhesives and Sealants Industry or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • Assembly automation for medical device manufacturing
    Sponsored byNordson EFD

    Three Proven Principles Powering Quality Assembly

Popular Stories

image of handshake

APPLIED Adhesives Expands Silicone Solutions and East Coast Presence with Acquisition

People shaking hands

Henkel Names Exclusive US Distributor for Flexible Packaging Technologies

Picture of a lobby of a Henkel facility

Henkel Expands Silicon Valley Application Center for Electronics

ASI 2026 Top 20 Adhesives & Sealants List

Events

September 15, 2026

Coatings Trends & Technologies Summit

This annual Midwest coatings conference combines all of the high-quality technical presentations, exhibits and networking opportunities from the Coatings Trends and Technologies and Powder Coating Summit conferences into one new event. The event caters to both liquid and powder coatings formulators and manufacturers.

September 16, 2026

World Adhesive & Sealant Conference (WAC) 2026

As the industry’s premier international event, WAC 2026 offers a unique opportunity for professionals from every continent to connect, collaborate, and shape the future of the sector.
View All Submit An Event

Products

Structural Adhesives: Properties, Characterization and Applications

Structural Adhesives: Properties, Characterization and Applications

See More Products

Related Articles

  • Photo of a handshake

    SOCMA Welcomes Eight New Members in 2022 First Half

    See More
  • SOCMA WELCOMES SEVEN NEW MEMBERS IN FOURTH QUARTER

    See More
  • Williams Elected Chair of SOCMA Board of Governors

    See More

Related Products

See More Products
  • thirdedition.jpg

    Handbook of Adhesive Technology, Third Edition

  • 9780080447087.jpg

    Volume 2: Handbook of Adhesives and Sealants, 1st Edition

See More Products

Related Directories

  • Society of Chemical Manufacturers & Affiliates (SOCMA)

    The Society of Chemical Manufacturers & Affiliates® (SOCMA) empowers our members with the latest industry knowledge, an unparalleled peer network, highly customized resources and dedicated technical and professional staff. As well as supports and fosters the growth of the specialty chemical industry by delivering legislative and regulatory advocacy, promoting the highest levels of safety, and strengthening business intelligence and manufacturing operations.
  • United Soybean Board

    United Soybean Board is a farmer-led organization that funds research to commercialize new industrial applications using chemical derivatives from U.S. Soy—including adhesive applications. USB-funded commercialization successes also include soy-based paints and coatings, polyurethane foam, composites and rubber products. Learn more about U.S. Soy's benefits including sustainability, quality and performance.
  • BASA

    BASA is an unincorporated trade association set up to act as the voice for the industry in the UK and Ireland. BASA supports its members by representing and promoting the industry, offering guidance on technical and compliance issues, providing networking opportunities for members, and providing members with support services.
×

Keep the info flowing with our newsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Manufacturing Division
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing