A new manufacturing process allows touchscreens to be flexible, curved, 3-D or wearable.
Heraeus recently announced that, in collaboration with the Industrial Technology Research Institute (ITRI), it has developed an improved mass-manufacturing process for its Clevios™-based films used in touch panels and sensors for a variety of electronics devices. This process will reportedly enable companies to use Clevios-based films to produce touchscreens with greater functionality, including the ability to be flexible, curved, 3-D or wearable.
Electronic devices are everywhere nowadays,―from the touchscreen checkout monitors at the local library and grocery store to car dashboard navigation systems and communications―applications that we wouldn’t have dreamed could exist just a couple decades ago.
The agreement reportedly covers the global rights related to the formulation and manufacturing process in addition to customer information to 11 solvent acrylic PSA products.